Microhardness nano and submicrostructure in coatings on solid carbide cutting tool

Free!

Category: .

Product Description

The results of studies on the relationship coating microhardness 0,18 HfN + 0,82 ZrNon cutting tools with carbide VK8, T15K6, MS221 and Sandvik Koromant and grain size (measured by REM-106). It was shown that growth of grain size leads to a reduction of microhardness, and for two-layer coating Al2O3 + (0,18 HfN + 0,82 ZrN) the microhardness is practically independent of time, to measure the grain nanostructured coating and decrease its value associated with the presence of the first layer Al2O3 having a lowest microhardness. Тransition from a nanostructured coating to submicrostructure loosed leads to a substantial decrease in microhardness.

Additional Information

Authors

Бруяка О.О., Костюк Г.И., Миргородская Е.В.

Year of publication

2014

6

Volume

113

Language

Russian

Types of files

pdf

Section

Ion Plasma Technologies and Equipment

Quality

excellent

Reviews

There are no reviews yet, would you like to submit yours?

Be the first to review “Microhardness nano and submicrostructure in coatings on solid carbide cutting tool”

Have an Ad? Submit it here!

*

*

*